Paraffin waxes for powder pressing need to be relatively hard in order to avoid premature blocking and to guarantee smooth pressing during production. We recommend our grades Sasolwax 5403, 5603 and 3501. For the production of tealights we have special grades such as Sasolwax 0986 and 5203.
We would be pleased to assist you with regard to your individual requirements.
|
DIN ISO 2207 ASTM D 938 |
DIN ISO 2908 ASTM D 721 |
DIN ISO 51579 ASTM D 1321 |
| 0155 |
54 - 56 |
0 - 1.2 |
21 - 26 |
|
5403 |
54 - 56 |
0 - 0.5 |
16 - 20 |
| 5603 |
56 - 58 |
0 - 0.5 |
15 - 19 |
|
5803 |
58 - 60 |
0 - 0.5 |
15 - 19 | We reserve the right to make changes to accord with further developments.
|