4. The Power of the Sasolwax Link TX Technology includes:
(a) Convenient to handle free-flowing powder form.
(b) Ease of dispersion
(c) Dispersion time is dramatically reduced from the usual 5 hours dispersion time (for SBS alone) to about 2 hours in total, further no post dispersion stabilization time is necessary.
(d) Since dispersion cycle times are minimized, Plant throughput is increased.
(e) The viscosity of the modified asphalt is substantially reduced such that it may be easily handled and transported with consequent energy savings.
(f) A stable modified asphalt blend is produced such that it is easy to handle, transport and use without the bother of phase separation and associated inconveniences.
(g) It is possible to produce a low viscosity co-modified concentrate (12.0% modifier loading) for ease of transportation to satellite locations for dilution to target PG.
5. Roofing Applications
Sasolwax Link TX is also recommended for roofing applications and has all of the benefits outlined above. The low viscosity improves workability substantially in both shingle and membrane applications and provides a higher capacity for fillers. Bleeding, deformation and high temperature wear is substantially reduced by the more effectively dispersed and cross-linked modifier system.
Since substantially higher polymer loading is employed in the Roofing Industry, Sasolwax Link TX provides significant savings through more effective Polymer cross-linking and reduced overall levels to meet target specifications.
(A). UV MICROGRAPH OF ASPHALT SAMPLE MODIFIED WITHOUT SASOLWAX LINK TX BUT A MIXTURE OF 1% SASOBIT AND 2% SBS
The micrograph below is that of an asphalt sample modified with 1% Sasobit and 2% SBS without the Cross-Linking agent i.e. without Sasolwax Link TX .
The mixing temperature was 350°F for 90 minutes using a Silverson high shear mixer.
The yellow fluorescent spots clearly highlight the SBS double bonds that are still intact i.e. no mechanism present to break the bonds and promote cross-linking.
(B). UV MICROGRAPH OF ASPHALT SAMPLE MODIFIED WITH SASOLWAX LINK TX
The micrograph below is that of an asphalt sample modified with Sasolwax Link TX .
The mixing temperature was 350° F for 90 minutes using a Silverson high shear mixer to be comparative with the experiment without Sasolwax Link TX .
The yellow fluorescent spots are no longer visible demonstrating that the double bonds on the SBS have been utilized to produce a complete network structure i.e. the SBS has been more effectively dispersed.